Revision history
2012/04/23: Initial release.
Notes from development: Increase duration of continuous wash. Consider switching to 1+3 developer dilution with 22 min. development time. Also consider reducing development time. Also, developer ended at 22°C.
2012/05/01: Increased continuous wash duration to 5 minutes. Added note to minimize handling of developer tank.
Notes from development: Started developer temp at 19.5° to allow for heating; ended at 21°C. Some artifacts along top edge of film ("top" relative to coiled cylinder inside the developing tank), see this example.